Steel Grade Equivalents: S235, S275 and S355 vs ASTM, JIS, GB and Other Standards
Published November 2026 · 9 min read · Technical Reference · Structural Steel
A drawing from Germany specifies S355J2, the supplier quotes ASTM A572 Grade 50, and the client's old standard still says St52-3. Are they the same steel? Close, but not exactly. This guide gives a cross-reference of structural steel grades across European, American, Japanese, Chinese, Indian, Canadian, Australian and Russian standards. It also explains the differences that matter when you substitute one grade for another, and includes a grade equivalent finder.
• S235JR ≈ ASTM A36 ≈ JIS SS400 ≈ GB Q235B ≈ old DIN St37-2.
• S275JR ≈ ASTM A572 Grade 42 ≈ old BS 4360 43A.
• S355J2 ≈ ASTM A572 Grade 50 / A992 ≈ JIS SM490B ≈ GB Q355B ≈ old DIN St52-3.
• The number in an EN grade is the minimum yield strength in MPa for thin sections. The letters show the impact test temperature.
• "Equivalent" means similar strength, not identical. Toughness, chemistry and thickness limits can differ.
How to Read a European Steel Grade
European structural grades follow EN 10027-1. Take S355J2+N as an example:
| Part | Meaning |
|---|---|
| S | Structural steel |
| 355 | Minimum yield strength in MPa for thicknesses up to 16 mm. It decreases for thicker products. |
| J2 | Impact energy of at least 27 J at −20 °C. JR = +20 °C, J0 = 0 °C, J2 = −20 °C. K2 = 40 J at −20 °C. |
| +N | Delivery condition: normalised or normalised rolled. +AR = as rolled, +M = thermomechanically rolled (EN 10025-4). |
Hollow sections add an "H" (S355J2H), and coated sheet uses "GD" (S350GD). See our guides to hollow sections and galvanized steel grades.
Grade Equivalent Finder
Grades are grouped by similar minimum yield strength. Values are for thin products (typically up to 16 mm). Check the full standard for thicker sections and other requirements.
Structural Steel Equivalents Table
Approx. 235–250 MPa class
| Grade | Standard | Region | Min. yield (MPa) | Tensile (MPa) | Impact test |
|---|---|---|---|---|---|
| S235JR | EN 10025-2 | Europe | 235 | 360–510 | 27 J at +20 °C |
| S235J2 | EN 10025-2 | Europe | 235 | 360–510 | 27 J at −20 °C |
| ASTM A36 | ASTM A36 | USA | 250 | 400–550 | Not required unless specified |
| SS400 | JIS G3101 | Japan | 245 | 400–510 | Not specified |
| SM400B | JIS G3106 | Japan | 245 | 400–510 | 27 J at 0 °C |
| Q235B | GB/T 700 | China | 235 | 370–500 | 27 J at +20 °C |
| E250 | IS 2062 | India | 250 | min. 410 | Depends on quality A/BR/B0/C |
| St3sp | GOST 380 | Russia/CIS | 245 | 370–480 | Depends on category |
| St37-2 | DIN 17100 (withdrawn) | Old German | 235 | 340–470 | Old name of S235JR |
Approx. 275–300 MPa class
| Grade | Standard | Region | Min. yield (MPa) | Tensile (MPa) | Impact test |
|---|---|---|---|---|---|
| S275JR | EN 10025-2 | Europe | 275 | 410–560 | 27 J at +20 °C |
| S275J2 | EN 10025-2 | Europe | 275 | 410–560 | 27 J at −20 °C |
| ASTM A572 Gr. 42 | ASTM A572 | USA | 290 | min. 415 | Not required unless specified |
| 300W | CSA G40.21 | Canada | 300 | 450–620 | Not required for W |
| Grade 300 | AS/NZS 3679.1 | Australia | 300 | min. 440 | L0 grades tested at 0 °C |
| 43A | BS 4360 (withdrawn) | Old British | 275 | 430–580 | Old name ~S275JR |
Approx. 345–355 MPa class
| Grade | Standard | Region | Min. yield (MPa) | Tensile (MPa) | Impact test |
|---|---|---|---|---|---|
| S355JR | EN 10025-2 | Europe | 355 | 470–630 | 27 J at +20 °C |
| S355J2 | EN 10025-2 | Europe | 355 | 470–630 | 27 J at −20 °C |
| S355K2 | EN 10025-2 | Europe | 355 | 470–630 | 40 J at −20 °C |
| ASTM A572 Gr. 50 | ASTM A572 | USA | 345 | min. 450 | Not required unless specified |
| ASTM A992 | ASTM A992 | USA | 345 | min. 450 | Not required unless specified; max. yield 450 MPa |
| SM490B | JIS G3106 | Japan | 325 | 490–610 | 27 J at 0 °C |
| Q355B | GB/T 1591 | China | 355 | 470–630 | 34 J at +20 °C |
| E350 | IS 2062 | India | 350 | min. 490 | Depends on quality |
| 350W | CSA G40.21 | Canada | 350 | 450–650 | Not required for W |
| Grade 350 | AS/NZS 3679.1 | Australia | 350 | min. 480 | L0 grades tested at 0 °C |
| 09G2S | GOST 19281 | Russia/CIS | 345 | min. 490 | Tested at −40 °C in higher categories |
| St52-3 | DIN 17100 (withdrawn) | Old German | 355 | 490–630 | Old name of S355J2 |
| 50D | BS 4360 (withdrawn) | Old British | 355 | 490–640 | Old name ~S355K2 |
Approx. 450–460 MPa class
| Grade | Standard | Region | Min. yield (MPa) | Tensile (MPa) | Impact test |
|---|---|---|---|---|---|
| S460M | EN 10025-4 | Europe | 460 | 540–720 | 40 J at −20 °C |
| ASTM A572 Gr. 65 | ASTM A572 | USA | 450 | min. 550 | Not required unless specified |
| SM570 | JIS G3106 | Japan | 460 | 570–720 | 47 J at −5 °C |
| Q460C | GB/T 1591 | China | 460 | 550–720 | 34 J at 0 °C |
Minimum yield strength for the thinnest thickness range; tensile strength ranges as given in the standards for common thicknesses. Values can differ between editions of a standard. This table is a guide for comparison, not a substitute for the specification.
Old Names You Will Still See
Many drawings and machines still carry withdrawn designations. The most common conversions are:
| Old designation | Old standard | Current EN grade | Material number |
|---|---|---|---|
| St37-2 | DIN 17100 | S235JR | 1.0038 |
| St37-3 | DIN 17100 | S235J2 | 1.0117 |
| St44-2 | DIN 17100 | S275JR | 1.0044 |
| St52-3 | DIN 17100 | S355J2 | 1.0577 (+N) |
| Fe 360 B | EN 10025:1990 | S235JR | 1.0038 |
| Fe 510 D1 | EN 10025:1990 | S355J2 | 1.0577 |
| 43A / 43C | BS 4360 | S275JR / S275J0 | 1.0044 / 1.0143 |
| 50B / 50D | BS 4360 | S355JR / S355K2 | 1.0045 / 1.0596 |
Why "Equivalent" Is Not "Identical"
Grades with the same strength can still behave differently. Check these five points before you accept a substitute:
Impact toughness
S355J2 guarantees 27 J at −20 °C. ASTM A572 Grade 50 and A36 have no impact test unless a supplementary requirement is ordered. For cold climates or dynamic loads, this difference matters.
Thickness dependence
EN grades lose yield strength in steps as thickness increases (S355 drops to 345 MPa above 16 mm). Other standards use different steps, so compare at the actual thickness.
Chemistry and weldability
Maximum carbon, CEV and impurity limits differ. A grade can match in strength and still need a different welding procedure. See our mill test certificate guide for the CEV check.
Upper yield limit
ASTM A992 limits the maximum yield strength and the yield-to-tensile ratio for seismic design. Most EN grades have no maximum yield. A stronger-than-specified steel is not always acceptable.
Documents and marking
CE marking under EN 1090 requires EN-certified products with 3.1 certificates. A steel that only meets an ASTM grade may not be acceptable on an EU project, and vice versa.
Substituting a Grade: A Practical Checklist
- Compare yield and tensile strength at the actual thickness, not only the grade name.
- Compare impact requirements: test temperature, energy and specimen direction.
- Check chemistry and CEV against the welding procedure qualified for the project.
- Check special requirements: through-thickness properties (Z grades), maximum yield, galvanizability (silicon and phosphorus).
- Check the documents: certificate type (EN 10204 3.1 or 3.2), CE marking, and project approval.
- Get written approval from the structural engineer or the client before you substitute.
Sourcing Structural Steel from Türkiye
Turkish mills produce structural sections, plates and hollow sections to EN 10025 and EN 10219, and many also certify to ASTM, JIS or other national standards for export markets. This makes Türkiye a convenient source for projects in Europe, the Middle East, Africa and the Americas. See our structural steel sections, and the size tables for HEA/HEB and IPE beams.
Frequently Asked Questions
What is the ASTM equivalent of S355J2?
The nearest ASTM equivalent is A572 Grade 50, or A992 for wide-flange beams. Both have a minimum yield strength of 345 MPa. S355J2 also guarantees 27 J impact energy at −20 °C, which the ASTM grades only provide if a supplementary impact test is ordered.
Is S235JR the same as ASTM A36?
They are close but not identical. S235JR has a minimum yield strength of 235 MPa and A36 has 250 MPa. S235JR requires an impact test at +20 °C, while A36 has no standard impact requirement. They are often treated as equivalent for general structural work.
What is the Chinese equivalent of S355?
The Chinese equivalent is Q355 to GB/T 1591, which replaced the older Q345. Q355B is tested at +20 °C, Q355C at 0 °C and Q355D at −20 °C, so Q355D is the closest match to S355J2.
What is the JIS equivalent of S235 and S355?
JIS SS400 or SM400 is broadly equivalent to S235, and SM490 is broadly equivalent to S355. Note that SS400 has no limits on carbon and impact properties, while the SM grades are weldable structural steels with tighter requirements.
What is St52-3 called today?
St52-3 from the old DIN 17100 corresponds to S355J2 (material number 1.0577) under EN 10025-2. St37-2 corresponds to S235JR.
Can I replace S355 with ASTM A572 Grade 50 on a European project?
Only with approval. The strength is similar, but the impact toughness, chemistry limits and certification differ, and CE marking under EN 1090 normally requires EN-certified material. Dual-certified steel that meets both standards avoids the problem.
Send your grade, standard and quantities. Steeling.net returns offers from Turkish mills for EN, ASTM and dual-certified structural steel with 3.1 certificates. There are no fees for buyers.
Get a Free Quote →